AA screen pattern containing a large number of low-level indications (often reffered toas ‘hash’) could be caused by: |
| A. | A crack |
| B. | A large inclusion |
| C. | Coarse grained material |
| D. | Fine grained material |
| Answer» D. Fine grained material | |