| 1. |
Match the following sand mold casting defects with their respective causes.DefectCauseP. Blow hole1. Poor collapsibilityQ. Misrun2. Mold erosionR. Hot tearing3. Poor permeabilityS. Wash4. Insufficient fluidity |
| A. | P-4, Q-3, R-1, S-2 |
| B. | P-3, Q-4, R-2, S-1 |
| C. | P-2, Q-4, R-1, S-3 |
| D. | P-3, Q-4, R-1, S-2 |
| Answer» E. | |